PMC:7143804 / 33142-33328
Annnotations
LitCovid-PubTator
Id | Subject | Object | Predicate | Lexical cue | tao:has_database_id |
---|---|---|---|---|---|
227 | 16-18 | Chemical | denotes | Au | MESH:D006046 |
228 | 23-25 | Chemical | denotes | Pt | MESH:D010984 |
LitCovid-PD-CLO
Id | Subject | Object | Predicate | Lexical cue |
---|---|---|---|---|
T214 | 123-127 | http://purl.obolibrary.org/obo/UBERON_0000473 | denotes | test |
LitCovid-PD-CHEBI
Id | Subject | Object | Predicate | Lexical cue | chebi_id |
---|---|---|---|---|---|
T215 | 16-18 | Chemical | denotes | Au | http://purl.obolibrary.org/obo/CHEBI_29287 |
T216 | 23-25 | Chemical | denotes | Pt | http://purl.obolibrary.org/obo/CHEBI_33364|http://purl.obolibrary.org/obo/CHEBI_75318 |
LitCovid-sentences
Id | Subject | Object | Predicate | Lexical cue |
---|---|---|---|---|
T257 | 0-186 | Sentence | denotes | The adhesion of Au and Pt deposited by either evaporation or DC magnetron sputtering is investigated using the Scotch tape test [60,61] before and after temperature cycling up to 100 °C. |