{"target":"https://pubannotation.org/docs/sourcedb/PMC/sourceid/5551755","sourcedb":"PMC","sourceid":"5551755","source_url":"https://www.ncbi.nlm.nih.gov/pmc/5551755","text":"From the analysis of the data in Table 8, it could be noticed that when increasing the amount of pillared clay (methods 12, 14 and 15), a slight reduction of surface area occurred, with the lowest surface area obtained by method 14 (179 m2/g). For methods 11, 13, and 16, where the pillaring agent was synthesized in the course of a day with a heating stage at 60 °C, the surface areas remained high, even when pillaring 50 g of clay (Figure 5).","tracks":[]}