PMC:4137170 / 6830-7332 JSONTXT

Annnotations TAB JSON ListView MergeView

{"target":"https://pubannotation.org/docs/sourcedb/PMC/sourceid/4137170","sourcedb":"PMC","sourceid":"4137170","source_url":"https://www.ncbi.nlm.nih.gov/pmc/4137170","text":"Porous β-tricalcium phosphate microsphere\nThe porous β-TCP (Cerectron Co., Kimpo, South Korea) microspheres were prepared by the spray-dry method. The resulting spherical particles were subsequently sintered at 1,250 °C for 2 h, resulting in diameters ranging from 45 to 75 μm (Fig. 1). The β-TCP that was sintered at high temperature had a porosity of 59.3 %, as measured with a mercury porosimeter.\nFig. 1 SEM images of β-TCP microspheres generated by the spray-dry method after sintering at 1,250 °C","divisions":[{"label":"title","span":{"begin":0,"end":41}},{"label":"label","span":{"begin":401,"end":407}}],"tracks":[]}