Test patterns consisting of rectangular metal strips of 2 mm by 14 mm are fabricated by depositing 100 nm of metal using a hand-made shadow mask made out of DuPont KaptonĀ® HN polyimide film of 0.05 mm thickness (RS Components B.V., Haarlem, The Netherlands).