Methods: 12 discs 15 mm in diameter and 2 mm thick were prepared from two shades (A2 & A4) of two composites, Durafil VS (DF) and TPH3 (TPH). Specimens were polished and stored in distilled water for 24 hours at 37°C before being subjected to bleaching, staining, and re-bleaching. Each of the groups of specimens (DF-A2, DF-A4, TPH-A2 and TPH-A4) were subdivided into three subgroups (n=4) and bleached with Beyond, LumaWhite-Plus, and Opalescence-Boost. Specimens were then stained by immersing them in a coffee solution for 48 hours at 37°C, and then they were re-bleached. Colorimetric measurements were performed at baseline, after bleaching, after staining, and after re-bleaching. Surface roughness was determined with environmental SEM before and after bleaching. Data were statistically-analyzed.